Alumina semi-Friable Fused adhibetur pro resina et vitrificata stridor rotarum cum summae superficiei peractivandi requisita, late laborantes in calore ferri sensitivo, mixtura, ferreum, instrumentum ferreum, ferrum missum, varia metalla non ferrea et chalybe immaculata. Instrumenta laesura ex eo aredurabilia, sui ipsius acuit et stabilis. Aspero stridor, processus efficiendi emendare potest. Ad subtilitatem stridor, potest emendare qualitatem superficiei workpiece.
Items | Unitas | Index | Typical | |
ChemicalComposition | Al2O3 | % | 96.50min | 97.10 |
SiO'2 | % | 1.00max | 0.50 | |
Fe2O3 | % | 0.30max | 0.17 | |
TiO2 | % | 1.40-1.80 | 1.52 | |
Compressive fortitudo | N | 26min | ||
lentitudo | % | 90.5 | ||
punctum liquescens | ℃ | 2050 | ||
Refractio | ℃ | 1850 | ||
Verum density | g/cm3 | 3.88min | ||
Mohs duritiem | --- | 9.00min | ||
AbrasiveGradus | FEPA | F12-F220 | ||
Color | --- | Gray |